It is made by smash method with special auxiliaries in normal temperature. The size is 80mesh and above. It has low as, even size , can can improve the process and dynamic performance of products. It can increase life and lower the cost. It is widely used in tire, medium/top-grade rubber products and others.
Technical indexes
Moisture, % |
≤1.20 |
Tensile strength
Mpa |
≥15 |
Elongation at failure, % |
≥500 |
Ash, % |
≤10.00 |
Acetone extract, % |
≤22.00 |
Sieving rate , % |
≥90 |
|